PVD + a-C:H
For demanding tribological applications to reduce friction, wear or torque.
Coating material: | a-C:H based |
Colour: | Black |
Coathing thickness [μm]: | 0.5-3 |
Coating temperature [°C]: | 300-500 |
Nanohardness according to ISO 14577 HIT [GPa]: | 15 ± 2 |
Coefficient of friction against steel (dry): | 0.05-0.1 |
Max. application temperature [°C]: | 300 |